TECHNET Archives

March 2007

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
Date:
Thu, 15 Mar 2007 07:36:09 -0500
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, [log in to unmask]
Content-Transfer-Encoding:
quoted-printable
Subject:
From:
X-cc:
In-Reply-To:
Content-Type:
text/plain;charset=iso-8859-1
MIME-Version:
1.0
Parts/Attachments:
text/plain (29 lines)
Hi Werner,
We know the parts are not in spec.It was obvious when they first arrived
they were not ENIG just by the gold colour plus the plating bars to the
outside world. I know how to check for the gold embrittlement - it is the
nickel I am trying to get a handle on. Regards Steve Kelly>
What you received is NOT ENIG. This has been a not uncommon problem with
> parts from China--they use an electrolytic Au-flash—I have seen
> Au-embrittlement
> as a consequence.
>
> Werner
>
>
>
> **************************************
>  AOL now offers free email to everyone.
>  Find out more about what's free from AOL at http://www.aol.com.
>

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2