TECHNET Archives

August 2002

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
Date:
Wed, 14 Aug 2002 16:22:35 +0200
Content-Disposition:
inline
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, "d. terstegge" <[log in to unmask]>
Subject:
MIME-Version:
1.0 (Generated by NET-TEL Mailguard SMTP version 4.0.0.22)
Content-Transfer-Encoding:
7bit
Content-Type:
text/plain; charset=US-ASCII
From:
"d. terstegge" <[log in to unmask]>
Parts/Attachments:
text/plain (27 lines)
Hi Brian,

Thanks for the clarification. The "good reason" for the lack of coating
on some areas of the IC's is that there seems to be a kind of dewetting
from these surfaces. The machine manufacturer's engineer told us that
this is quite normal, and is caused by release agents that are used
during manufacturing of the IC's.
To have nicer results (or have the extra 18 days of damage-prevention)
it seems that manual rework is needed.
B.T.W. it's great to have you back on this forum, it certainly enhances
the technical relevance of many discussions !

Daan Terstegge
Unclassified mail
Personal Website: http://www.smtinfo.net

---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------

ATOM RSS1 RSS2