Have no idea what strange things you are doing, but an easy way to activate
the copper is to dip the boards in a weak acid solution, strength depending
on the time the boards have been exposed to the atmosphere. Rinse rigorously
in DI !
/Inge
-----Ursprungligt meddelande-----
Från: TechNet [mailto:[log in to unmask]] För Ioan Tempea
Skickat: den 19 mars 2008 13:42
Till: [log in to unmask]
Ämne: [TN] Shelf lif of bare copper boards
Dear Technos,
Anybody using PCbs with bare copper pads and traces, no plating, no OSP,
not even solder mask? Because I have a few questions:
What is their shelf life?
Are they suited for double side SMT reflow? I mean, during the first
reflow the oxidizing is accelerated...
What storing/handling procedures you use?
Does the copper require any particular specifications, in order to
perform better in soldering?
Anything else?
Thank you,
Ioan
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|