TECHNET Archives

November 2008

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>
Date:
Fri, 28 Nov 2008 08:56:21 -0800
Reply-To:
Subject:
From:
henry rekers <[log in to unmask]>
Content-Transfer-Encoding:
quoted-printable
In-Reply-To:
Content-Type:
text/plain; charset=iso-8859-1
MIME-Version:
1.0
Parts/Attachments:
text/plain (113 lines)
I'll try to get some pictures today.  It is a very strange behavior.  We are seeing everything in spec from the board vendors (thickness/P content) and we are seeing everything in spec in the wave process, flux, alloy, profile.  But, we still get these dewets.  We've seen it on selective and standard wave from at least two different board shops using two different chemistries.  It has been suggested that decreasing dwell time, or using more agressive flux may help, but I hesitate to make major changes in an established process without knowing what the root cause is.  We're spending a lot of bucks on lab work, so I was hoping to collaborate with anyone else that is having this issue.  I've heard rumors that an oem on the east coast had the same issues?
 
Apparently the plating committee and the enig suppliers have been looking at this and it is described as a bit of an epidemic and they are calling it a new phenomenon that could rival black pad.  I would just like to find out more.
 
Thanks.

--- On Fri, 11/28/08, David D. Hillman <[log in to unmask]> wrote:

From: David D. Hillman <[log in to unmask]>
Subject: Re: [TN] nickel erosion
To: [log in to unmask]
Received: Friday, November 28, 2008, 10:39 AM

Hi Henry! Wow, nickel plating is commonly used as a barrier layer in a 
number of electronics applications so having an erosion issue would be 
somewhat odd. I would expect that a lead-free soldering process would 
remove more nickel (either thru erosion or dissolution) in comparison to a 
tin/lead soldering process due to the increased process temperatures but 
what you are describing (large?) sounds strange. Have you compared the 
nickel thickness pre and post soldering process? Do you have any 
microsection photos Steve could post so we could get a look at the 
situation? I have run a significant number of ENIG pwbs thru both 
lead-free wave and reflow processes but have not seen the condition you 
describe. Are you on a mini-wave, selective solder or typical wave solder 
system?

Dave Hillman
Rockwell Collins
[log in to unmask]




henry rekers <[log in to unmask]> 
Sent by: TechNet <[log in to unmask]>
11/26/2008 06:17 PM
Please respond to
[log in to unmask]


To
[log in to unmask]
cc

Subject
[TN] nickel erosion






Any technetters out there experiencing this mysterious nickel erosion 
process with enig boards on their leadfree waves?  Apparently there is a 
committee set up already.  I would like to share experiences if anyone is 
willing to come forward.
 
Essentially, the defect shows up as a dewet on the annular ring of the TH 
devices.  On cross section, there is large amounts of nickel eroded away 
and the surface is non-wettable.  No corrosion is evident, so it's NOT 
black pad.
 
Anybody?


      __________________________________________________________________
Instant Messaging, free SMS, sharing photos and more... Try the new Yahoo! 
Canada Messenger at http://ca.beta.messenger.yahoo.com/

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to 
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to 
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 
for additional information, or contact Keach Sasamori at [log in to unmask] or 
847-615-7100 ext.2815
-----------------------------------------------------


---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------



      __________________________________________________________________
Connect with friends from any web browser - no download required. Try the new Yahoo! Canada Messenger for the Web BETA at http://ca.messenger.yahoo.com/webmessengerpromo.php

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2