Stress releif baking needs to be done above the Tg for the material. Most
would hold at that temperature for 4 hours min. The cool down rate is
critical because of the various CTEs of the laminate constituents (glass,
epoxy, copper). Somewhere around 4 deg/min F back thru the Tg is usually
what's recommended.
Bob Dube
-----Original Message-----
From: Timothy Reeves <[log in to unmask]>
To: [log in to unmask] <[log in to unmask]>
Date: Friday, March 24, 2000 12:56 PM
Subject: [TN] laminate stress relief
Good Day, TechNet!
board fabs: what (if any) baking of incoming core material do you do to
minimize movement of layers. We try to have the material at 250°F for one
hour based on what someone told us quite a while back. Without going through
a big DOE, I'd like to ascertain if that's enough.
Danke schön.
Timothy Reeves
ECD Circuit Board Division
13626 South Freeman Road
Mulino, OR 97042
[log in to unmask]
(503) 829-9108 (800) 228-8198 FAX (503) 829-5482
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following
text in
the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
##############################################################
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
##############################################################
|
|
|