David Fish <[log in to unmask]>
Reply To:
TechNet E-Mail Forum.
Date:
Tue, 14 Aug 2001 21:31:59 -0700
Content-Type:
text/plain
Parts/Attachments:
text/plain (58 lines)
RJ Klien Wassink suggests [bible p 169] pouring contaminated solder at about
190°C through a 20 mesh stainless steel stariner to reduce copper content to
0.25%.

Dave Fish
----- Original Message -----
From: "Phil Nutting" <[log in to unmask]>
To: <[log in to unmask]>
Sent: Tuesday, August 14, 2001 5:48 AM
Subject: [TN] Solder analysis results


> Ok folks, here is today's question.
>
> I just received a Certificate of Analysis (our first one) for the solder
> in our Soltec Waver Solder machine.  All parameters are "within
> specification" except the percentage of copper which is at 1.6859. (Tin
> is at 61.3% and Lead is at 36.99% and other stuff is at 0.0199%)  We run
> 63/37 in the wave.  We only solder our own product, none of which goes
> into "mission critical" applications.  We normally build our product to
> IPC-A-610C, Class 2.
>
> My question is two-fold.  Should I worry about this?  If so, how do I
> fix it with 1700 pounds of solder in the solder pot?
>
> Thanks is advance for sharing your knowledge.
>
> Phil Nutting
> Manufacturing Engineer
> Kaiser Systems, Inc.
>
> --------------------------------------------------------------------------
-------
> Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt delivery of Technet send the following message: SET
Technet NOMAIL
> Search previous postings at: www.ipc.org > On-Line Resources & Databases >
E-mail Archives
> Please visit IPC web site (http://www.ipc.org/html/forum.htm) for
additional
> information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
> --------------------------------------------------------------------------
-------
>

---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------

ATOM RSS1 RSS2