TECHNET Archives

November 2010

TechNet@IPC.ORG

Options: Use Proportional Font
Show HTML Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
Steve Gregory <[log in to unmask]>
Reply To:
TechNet E-Mail Forum <[log in to unmask]>, Steve Gregory <[log in to unmask]>
Date:
Tue, 16 Nov 2010 13:39:02 -0500
Content-Type:
text/plain
Parts/Attachments:
text/plain (161 lines)
I think Chuck is right, a cross section is needed, and I also think he is
right when he says it may reveal bad news.

I noticed something else in the picture. Look at the barrel walls of the
larger through-holes to right around TP7 and the ones above it. I know the
vias are a different diameter than those holes, but if the barrel walls in
those hole are an indicator of the quality of the holes in the rest of the
board, then that's not good...

Steve

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Chuck Brummer
Sent: Tuesday, November 16, 2010 1:14 PM
To: [log in to unmask]
Subject: Re: [TN] Radially discoloration on solder-resist covered via holes,
why?

Charming,

I think you need a micro section and it will reveal bad news.  Rudy may be 
right or there may be an internal separation.  Is this a multi layer?  I 
once saw a set of boards on which they spend to much time in the glass 
etch and when copper plating the holes the copper wicked up the glass 
fibers. 

 Chuck Brummer l 3M Manufacturing Engineer
3m Electronic Solutions Division--Flexible Circuits
8357 Canoga Ave. l Canoga Park, CA 91304-2605
(818) 734-4930
[log in to unmask] l www.3m.com l www.3mFlex.com




From:
Steve Gregory <[log in to unmask]>
To:
<[log in to unmask]>
Date:
11/16/2010 08:48 AM
Subject:
Re: [TN] Radially discoloration on solder-resist covered via holes, why?
Sent by:
TechNet <[log in to unmask]>



Hi Charming,

 

I have your picture posted, it's here:

 

http://stevezeva.homestead.com/Pic1.JPG

 

Maybe they weren't cleaned well before solder masking?

 

Steve

 

From: Charming Chan [mailto:[log in to unmask]] 
Sent: Tuesday, November 16, 2010 10:51 AM
To: [log in to unmask]
Subject: Radially discoloration on solder-resist covered via holes, why?

 

Hi Steve,

Would you help post the attached picture for me and forward this message 
to
TechNet? Thanks a lot.

 

The picture shows radially discoloration on solder-resist covered via 
holes,
while, the immersion silver pads without solder-paste reflowing have shiny
appearance with no discoloration. With naked eye checking, the 
discoloration
on solder-resist covered via holes is not corrosion product.

 

BTW, the pcb board surface finish is immersion silver, via holes are fully
pluged with solder resist, and no discoloration is observed after pcb
assembly finished. The discoloration possibly gets start in PCBA 
storaging.

Best Regarads

Charming Chan



______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to 
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to 
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 
for additional information, or contact Keach Sasamori at [log in to unmask] or 
847-615-7100 ext.2815
-----------------------------------------------------





______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------


______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2