Right you are, the polyurethane will break down. But you can send a urethane coated board through wave solder and the coat survive that short duration. Yes I had to do that once. The coat acted as a selective soldering fixture. And no I do not recomend this as a common practice. Just sometimes we gotta do some strange things to get the job done.
-----Original Message-----
From: Dave Hillman [mailto:[log in to unmask]]
Sent: Friday, July 19, 2002 7:59 AM
To: [log in to unmask]
Subject: Re: [TN] Solder Pot Contamination
Hi Mike! This is more of a question than a statement but would not
polyurethane particles char/burn/decompose if immersed in the wave
solderpot and end up being a constituent of the solderpot dross? I couldn't
find the char/flame resistance values for polyurethane but I am guessing
that they would not survive long in the solderpot (typical solderpot
temperature = 500F).
Dave Hillman
Rockwell Collins
[log in to unmask]
Michael Bell <[log in to unmask]>@ipc.org> on 07/18/2002 09:37:05 PM
Please respond to "TechNet E-Mail Forum." <[log in to unmask]>; Please respond
to Michael Bell <[log in to unmask]>
Sent by: TechNet <[log in to unmask]>
To: [log in to unmask]
cc:
Subject: [TN] Solder Pot Contamination
Hi all,
Has anyone ever come across a method in which to detect resin (polyurethane
particles) contamination in a Wave Solder Pot???? And in turn, a method to
remove this sort of contamination???
Cheers
Mike
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
---------------------------------------------------------------------------------
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|