TechNet E-Mail Forum <[log in to unmask]>, David Tremmel <[log in to unmask]>
Date:
Wed, 8 Mar 2006 17:51:21 -0500
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Joe Russeau <[log in to unmask]>
Subject:
MIME-Version:
1.0
Content-Transfer-Encoding:
quoted-printable
Content-Type:
text/plain; charset="iso-8859-1"
From:
Joe Russeau <[log in to unmask]>
Parts/Attachments:
text/plain (142 lines)
Nauga chance!!!

Joe Russeau

----- Original Message -----
From: "David Tremmel" <[log in to unmask]>
To: <[log in to unmask]>
Sent: Wednesday, March 08, 2006 5:47 PM
Subject: Re: [TN] NTC : ESD and paintbrushes - nauga farms


> I wonder if some of those on Technet would wish we would just naug it off?
> :)
>
>
> David
>
>
> >From: Joe Russeau <[log in to unmask]>
> >Reply-To: TechNet E-Mail Forum <[log in to unmask]>,              Joe
Russeau
> ><[log in to unmask]>
> >To: [log in to unmask]
> >Subject: Re: [TN] NTC : ESD and paintbrushes - nauga farms
> >Date: Wed, 8 Mar 2006 17:38:00 -0500
> >
> >Dewey,
> >
> >Don't nauga, till u try-a!
> >
> >Joe Russeau
> >
> >----- Original Message -----
> >From: "Whittaker, Dewey (AZ75)" <[log in to unmask]>
> >To: <[log in to unmask]>
> >Sent: Wednesday, March 08, 2006 5:28 PM
> >Subject: Re: [TN] NTC : ESD and paintbrushes - nauga farms
> >
> >
> > > 8 miles high in a Lead-Free Airplane. Now that is for the Byrds.
> > > Dewey
> > >
> > > -----Original Message-----
> > > From: TechNet [mailto:[log in to unmask]] On Behalf Of Joe Fjelstad
> > > Sent: Wednesday, March 08, 2006 3:19 PM
> > > To: [log in to unmask]
> > > Subject: Re: [TN] NTC : ESD and paintbrushes - nauga farms
> > >
> > > Joe did  always think he was hot stuff....
> > >
> > >
> > >
> > > Oooo, ouch, oooo, ooo, ouch... I am on fire here...  ;-)
> > >
> > > Paraphrasing the Byrds:
> > >
> > > To everything there is flash point, Burn, burn, burn... :-)
> > >
> > > Smokin' Joe
> > >
> > >
> > > ---------------------------------------------------
> > > Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
> > > unsubscribe, send a message to [log in to unmask] with following text in
> > > the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt
or
> > > (re-start) delivery of Technet send e-mail to [log in to unmask]: SET
> > > Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
> > > posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
> > > archives of previous posts at: http://listserv.ipc.org/archives Please
> > > visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for
> > > additional information, or contact Keach Sasamori at [log in to unmask] or
> > > 847-615-7100 ext.2815
> > > -----------------------------------------------------
> > >
> > > ---------------------------------------------------
> > > Technet Mail List provided as a service by IPC using LISTSERV 1.8e
> > > To unsubscribe, send a message to [log in to unmask] with following text
> >in
> > > the BODY (NOT the subject field): SIGNOFF Technet
> > > To temporarily halt or (re-start) delivery of Technet send e-mail to
> >[log in to unmask]: SET Technet NOMAIL or (MAIL)
> > > To receive ONE mailing per day of all the posts: send e-mail to
> >[log in to unmask]: SET Technet Digest
> > > Search the archives of previous posts at:
> >http://listserv.ipc.org/archives
> > > Please visit IPC web site
> >http://www.ipc.org/contentpage.asp?Pageid=4.3.16
> >for additional information, or contact Keach Sasamori at [log in to unmask]
or
> >847-615-7100 ext.2815
> > > -----------------------------------------------------
> > >
> > >
> >
> >---------------------------------------------------
> >Technet Mail List provided as a service by IPC using LISTSERV 1.8e
> >To unsubscribe, send a message to [log in to unmask] with following text in
> >the BODY (NOT the subject field): SIGNOFF Technet
> >To temporarily halt or (re-start) delivery of Technet send e-mail to
> >[log in to unmask]: SET Technet NOMAIL or (MAIL)
> >To receive ONE mailing per day of all the posts: send e-mail to
> >[log in to unmask]: SET Technet Digest
> >Search the archives of previous posts at:
http://listserv.ipc.org/archives
> >Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16
> >for additional information, or contact Keach Sasamori at [log in to unmask]
or
> >847-615-7100 ext.2815
> >-----------------------------------------------------
>
> _________________________________________________________________
> Latinos en EE.UU: noticias y artículos de interés para ti
> http://latino.msn.com/noticias/latinoseneeuu
>
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 1.8e
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
> Search the archives of previous posts at: http://listserv.ipc.org/archives
> Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
> -----------------------------------------------------
>

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2