Michael -
This link shows the TC 91 committee structure. I am not sure which working group addresses the issue of gold in solder joints. However, I would suspect one of the two Working Groups on test methods. It appears to me the entire TC 91 is meeting in Berlin in October this year. This site lists some meetings in San Jose, USA last year, which I know they held. Also, there were some subcommittee meetings in Grenoble, France in May, which coincided with JISSO meetings, ,which I attended by teleconference. However, this gold in solder is probably not an active item right now, but I don't know. Do you know Walter Huck - I think of Murata, in Germany? I think he is very active in IEC actvities. There is also a link to Dieter Bergman of the US IPC, and he will know for sure the Berlin agenda.
http://www.iec.ch/dyn/www/f?p=102:7:0::::FSP_ORG_ID:1286
Denny Fritz
-----Original Message-----
From: Jeremias, Michael <[log in to unmask]>
To: [log in to unmask]
Sent: Tue, Aug 4, 2009 4:09 am
Subject: [TN] FORMULA FOR DETERMINING GOLD PERCENTAGE IN A SOLDER JOINT
Unfortunately, the discussion about the matter is not so serious as the
roblem.
Proceedings in technological quality are not available by (hundreds!) of
ails with ridiculous content but by hard work.
, Who knows the responsible at IEC or TC91, who is able to change it?
. Who is able to make thebchange request?
incerly
Michael Jeremias
ndustrial Engineering (OPPI41)
lectronics Production
(( Defence Electronics
ADS Deutschland GmbH
9077 Ulm
el.: +49 (0) 7 31.3 92-5533
ax: +49 (0) 7 31.3 92-73 15
-Fax: +49 (0) 7 31.3 92-20 5533
Before printing, think about the environment !
mailto: [log in to unmask]
ADS Deutschland GmbH
egistered Office: Ottobrunn
istrict Court of Munich HRB 107 648
hairman of the Supervisory Board: Dr. Thomas Enders
anaging Directors: Dr. Stefan Zoller (chairman), Michael Hecht
his E-mail and any attachment(s) to it are for the addressee's use only.
t is strictly confidential and may contain legally privileged information. No
onfidentiality or privilege is waived or lost by any mistransmission.
f you are not the intended addressee, then please delete it from your system
nd notify the sender immediateley. You are hereby notified that any use,
isclosure, copying or any action taken in reliance on it is strictly prohibited
nd may be unlawful. - Thank you.
-----Ursprüngliche Nachricht-----
on: TechNet [mailto:[log in to unmask]] Im Auftrag von Joyce Koo
esendet: Freitag, 31. Juli 2009 19:06
n: [log in to unmask]
etreff: Re: [TN] AW: [TN] AW: [TN] FORMULA FOR DETERMINING GOLD PERCENTAGE IN A
OLDER JOINT
Who ever made doc and approved it should get shot at... seriously. Not a Friday
oke.
-----Original Message-----
rom: TechNet [mailto:[log in to unmask]] On Behalf Of Jeremias, Michael
ent: Friday, July 31, 2009 12:17 PM
o: [log in to unmask]
ubject: [TN] AW: [TN] AW: [TN] FORMULA FOR DETERMINING GOLD PERCENTAGE IN20A
OLDER JOINT
Unfortunately it is not (!) a typo from me . The document DIN EN 61191-1
ontains this value 2,5 µm . But I am not confident, that this is low
nough for any process cases so we use for PTH the same rule as above as
entioned below
incerely
Michael Jeremias
-----Ursprüngliche Nachricht-----
on: TechNet [mailto:[log in to unmask]] Im Auftrag von Joyce Koo
esendet: Donnerstag, 30. Juli 2009 12:22
n: [log in to unmask]
etreff: Re: [TN] AW: [TN] FORMULA FOR DETERMINING GOLD PERCENTAGE IN A SOLDER
OINT
Must be a typo. Should be 0.25 micron? 10 micro-inches?
-------------------------
ent using BlackBerry
---- Original Message -----
rom: TechNet <[log in to unmask]>
o: [log in to unmask] <[log in to unmask]>
ent: Thu Jul 30 04:26:14 2009
ubject: [TN] AW: [TN] FORMULA FOR DETERMINING GOLD PERCENTAGE IN A SOLDER JOINT
IEC 61191-1
hapter 6.2.2 contains the rules
1,4% Volume Au, < 3% Wt Au in the final solder interconnection
2,5 µm for PTH Wave soldering (I am not confident, that this is low enough
or any process cases so we use for PTH the same rule as above)
You have to take into consideration solder paste volume(stencil-thickness),
etted Au-surface, wetted Au thickness
Own investigations show, that Au brittelness may occure from 1,6% Vol and
eally will occure from 2,3% Vol.
Sincerly
Michael Jeremias
ndustrial Engineering (OPPI41)
lectronics Production
(( Defence Electronics
ADS Deutschland GmbH
9077 Ulm
el.: +49 (0) 7 31.3 92-
5533
ax: +49 (0) 7 31.3 92-73 15
-Fax: +49 (0) 7 31.3 92-20 5533
Before printing, think about the environment !
mailto: [log in to unmask]
ADS Deutschland GmbH
egistered Office: Ottobrunn
istrict Court of Munich HRB 107 648
hairman of the Supervisory Board: Dr. Thomas Enders Managing Directors: Dr.
tefan Zoller (chairman), Michael Hecht This E-mail and any attachment(s) to it
re for the addressee's use only.
t is strictly confidential and may contain legally privileged information. No
onfidentiality or privilege is waived or lost by any mistransmission.
f you are not the intended addressee, then please delete it from your system
nd notify the sender immediateley. You are hereby notified that any use,
isclosure, copying or any action taken in reliance on it is strictly prohibited
nd may be unlawful. - Thank you.
---------------------------------------------------
echnet Mail List provided as a service by IPC using LISTSERV 15.0 To
nsubscribe, send a message to [log in to unmask] with following text in the BODY
NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start)
elivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or
MAIL) To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest Search the archives of previous posts at:
ttp://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
or additional information, or contact Keach Sasamori at [log in to unmask] or
47-615-7100 ext.2815
-------
---------------------------------------------
---------------------------------------------------------------------
his transmission (including any attachments) may contain confidential
nformation, privileged material (including material protected by the
olicitor-client or other applicable privileges), or constitute non-public
nformation. Any use of this information by anyone other than the intended
ecipient is prohibited. If you have received this transmission in error, please
mmediately reply to the sender and delete this information from your system.
se, dissemination, distribution, or reproduction of this transmission by
nintended recipients is not authorized and may be unlawful.
---------------------------------------------------
echnet Mail List provided as a service by IPC using LISTSERV 15.0 To
nsubscribe, send a message to [log in to unmask] with following text in the BODY
NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start)
elivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or
MAIL) To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest Search the archives of previous posts at:
ttp://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
or additional information, or contact Keach Sasamori at [log in to unmask] or
47-615-7100 ext.2815
----------------------------------------------------
---------------------------------------------------
echnet Mail List provided as a service by IPC using LISTSERV 15.0 To
nsubscribe, send a message to [log in to unmask]
0with following text in the BODY
NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start)
elivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or
MAIL) To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest Search the archives of previous posts at:
ttp://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
or additional information, or contact Keach Sasamori at [log in to unmask] or
47-615-7100 ext.2815
----------------------------------------------------
---------------------------------------------------------------------
his transmission (including any attachments) may contain confidential
nformation, privileged material (including material protected by the
olicitor-client or other applicable privileges), or constitute non-public
nformation. Any use of this information by anyone other than the intended
ecipient is prohibited. If you have received this transmission in error, please
mmediately reply to the sender and delete this information from your system.
se, dissemination, distribution, or reproduction of this transmission by
nintended recipients is not authorized and may be unlawful.
---------------------------------------------------
echnet Mail List provided as a service by IPC using LISTSERV 15.0 To
nsubscribe, send a message to [log in to unmask] with following text in the BODY
NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start)
elivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or
MAIL) To=2
0receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest Search the archives of previous posts at:
ttp://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
or additional information, or contact Keach Sasamori at [log in to unmask] or
47-615-7100 ext.2815
----------------------------------------------------
---------------------------------------------------
echnet Mail List provided as a service by IPC using LISTSERV 15.0
o unsubscribe, send a message to [log in to unmask] with following text in
he BODY (NOT the subject field): SIGNOFF Technet
o temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
o receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
earch the archives of previous posts at: http://listserv.ipc.org/archives
lease visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
dditional information, or contact Keach Sasamori at [log in to unmask] or
47-615-7100 ext.2815
----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|