Julie
The compatibility of coatings and masks is always a subject of doubt
unless you use similar chemistry for both. In my book, I recommended not
to use a solder mask if you intend to coat, provided you can get away
with it. Certainly, "no-clean" fluxes require compatible masks and this
is a subject for qualification testing: also on the degree of cure of
the mask. As a general rule (but not absolute), the order of quality of
masks are: (worst) dry film, LPI and UV screenable, 1-component
screenable and 2 component screenable (best). BTW I do not recommend
coating on top of "no-clean" residues, except under very specific
circumstances where the residues form part of the polymerisation
reaction chain -- and even then ...
Brian
Julie Dixon wrote:
>
> Dear Net,
>
> Has anyone ever heard of a problem with adhesion of conformal coating being
> caused from UV soldermask? Will no-clean fluxes at assembly plants react
> differently to different types of soldermasks or LPI?
>
> Thanks,
> Julie Dixon
>
> ##############################################################
> TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
> ##############################################################
> To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
> the body:
> To subscribe: SUBSCRIBE TECHNET <your full name>
> To unsubscribe: SIGNOFF TECHNET
> ##############################################################
> Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
> information.
> If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
> 847-509-9700 ext.5365
> ##############################################################
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
847-509-9700 ext.5365
##############################################################
|
|
|