TECHNET Archives

November 1999

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
Date:
Fri, 19 Nov 1999 09:48:53 +0200
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, Brian Ellis <[log in to unmask]>
Subject:
MIME-Version:
1.0
Content-Transfer-Encoding:
7bit
Content-Type:
text/plain; charset=us-ascii
From:
Brian Ellis <[log in to unmask]>
Parts/Attachments:
text/plain (55 lines)
Julie

The compatibility of coatings and masks is always a subject of doubt
unless you use similar chemistry for both. In my book, I recommended not
to use a solder mask if you intend to coat, provided you can get away
with it. Certainly, "no-clean" fluxes require compatible masks and this
is a subject for qualification testing: also on the degree of cure of
the mask. As a general rule (but not absolute), the order of quality of
masks are: (worst) dry film, LPI and UV screenable, 1-component
screenable and 2 component screenable (best). BTW I do not recommend
coating on top of "no-clean" residues, except under very specific
circumstances where the residues form part of the polymerisation
reaction chain -- and even then ...

Brian

Julie Dixon wrote:
>
> Dear Net,
>
> Has anyone ever heard of a problem with adhesion of conformal coating being
> caused from UV soldermask? Will no-clean fluxes at assembly plants react
> differently to different types of soldermasks or LPI?
>
> Thanks,
> Julie Dixon
>
> ##############################################################
> TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
> ##############################################################
> To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
> the body:
> To subscribe:   SUBSCRIBE TECHNET <your full name>
> To unsubscribe:   SIGNOFF TECHNET
> ##############################################################
> Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
> information.
> If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
> 847-509-9700 ext.5365
> ##############################################################

##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe:   SUBSCRIBE TECHNET <your full name>
To unsubscribe:   SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
847-509-9700 ext.5365
##############################################################

ATOM RSS1 RSS2