Sender: |
|
X-To: |
|
Date: |
Thu, 19 Apr 2007 14:28:50 -0400 |
Reply-To: |
|
Subject: |
|
From: |
|
X-cc: |
|
In-Reply-To: |
|
Content-Type: |
text/plain; charset="US-ASCII" |
MIME-Version: |
1.0 |
Parts/Attachments: |
|
|
Like a Swiss Watch????
Kerry McMullen
Principal New Product Mfg. Engineer
LTX Corporation
825 University Avenue
Norwood, MA 02062-2643
(T) 781-467-5468
(C) 508-631-1832
(F) 781-461-0993
Joe Fjelstad <[log in to unmask]>
Sent by: TechNet <[log in to unmask]>
04/19/2007 02:19 PM
Please respond to
TechNet E-Mail Forum <[log in to unmask]>; Please respond to
[log in to unmask]
To
[log in to unmask]
cc
Subject
[TN] Fragility of Pb-free Solder Joints
This just came in my email from SMT Net. I have not been able to link to
the
article yet but the title and first paragraph sounds familiar.
Joe
_Fragility of Pb-free Solder Joints_
(http://www.smtnet.com/adsystem/redir.cfm?adid=831)
_Universal Instruments_
(
http://www.smtnet.com/company/index.cfm?fuseaction=view_company&company_id=46383
)
Credit/Source: Peter Borgesen, Surface Mount Laboratory, Universal
Instruments; and Donald W. Henderson, IBM Corporation
Recent investigations have revealed that Pb-free solder joints may be
fragile, prone to premature interfacial failure particularly under shock
loading,
as initially formed or tend to become so under moderate thermal aging.
Depending on the solder pad surface finish, different mechanisms are
clearly
involved, but none of the commonly used surface finishes appear to be
consistently
immune to embrittlement processes. This is of obvious concern for
products
facing relatively high operating temperatures for protracted times and/or
mechanical shock or strong vibrations in service...
************************************** See what's free at
http://www.aol.com.
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|