I've heard of using silver based solder when you have a gold finish PCB like
an ENIG finish, although I'm not clear on exactly why to use it for that.
We don't use that finish.
The only situation that we use 2% silver solder is for boards which have
some ceramic resonator components installed that have a silver finish on
them. This will avoid having the silver leach off the component and into
the solder.
-----Original Message-----
From: Larry Koens [mailto:[log in to unmask]]
Sent: July 25, 2001 2:10 PM
To: [log in to unmask]
Subject: [TN] solder paste with 2% silver
Got a question for everyone,
I just switched companies and the new company that I'm with now uses a
62/36/2 solder paste. I've always used the 63/37 formula. The guys who
decided to use the 2% silver are no longer with the company. My question
to you is, why would they want the 2% silver in the paste? They know
something I don't?!
Thanks,
Larry
----------------------------------------------------------------------------
-----
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET
Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases >
E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
----------------------------------------------------------------------------
-----
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|