TECHNET Archives

December 2012

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
"Gervascio, Thomas L" <[log in to unmask]>
Reply To:
TechNet E-Mail Forum <[log in to unmask]>, Gervascio, Thomas L
Date:
Tue, 18 Dec 2012 17:42:46 +0000
Content-Type:
text/plain
Parts/Attachments:
text/plain (30 lines)
I had some made up from Stone Mountain Tool. It was a composite material that was laser cut- it was not cheap but it has held up to two years of repeated washings through a saponified wash. Contact me off line for more information if you desire.

Regards
Tom

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Richard Kraszewski
Sent: Tuesday, December 18, 2012 10:33 AM
To: [log in to unmask]
Subject: EXTERNAL: [TN] Source of ESD Mats Suitable for in-line wash baskets

Does anyone have a source for soft polymer ESD grid mats (similar to screening but with ~ 1 inch openings) that would be suitable to go through an inline wash system?

The function of these mats would be to serve as a cushion to the bottom side SMT components as they get shifted by the wash jets. 

Finding them ESD safe (safer/safe-ish ) is the challenge. 

Thanks in advance. 

Rich  Kraszewski/PLEXUS

______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________

______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

ATOM RSS1 RSS2