TECHNET Archives

April 2013

TechNet@IPC.ORG

Options: Use Monospaced Font
Show HTML Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
Guy Ramsey <[log in to unmask]>
Reply To:
TechNet E-Mail Forum <[log in to unmask]>, Guy Ramsey <[log in to unmask]>
Date:
Fri, 12 Apr 2013 12:25:41 -0400
Content-Type:
text/plain
Parts/Attachments:
text/plain (61 lines)
They keep improving these materials, so my experience might be made obsolete
by time. Beginning in about 1993 we treated our stockroom, cement on grade,
with S.D. epoxy paint. 
We had to refresh the surface every three or four years because it began to
peel and wear through in high traffic areas.  It performed well, was easy to
clean and lowered the amount of dust in the stockroom. Untreated concrete is
dusty.  It was short lived compared to tile or carpet, but much lower
maintenance that tile. 

Guy

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Steve Gregory
Sent: Thursday, April 11, 2013 12:05 PM
To: [log in to unmask]
Subject: [TN] Static dissapative epoxy floor coating

Morning All,

 

Does anybody have any feedback on this static dissipative epoxy floor
coating? I've never used it before and was wondering how it performs in real
life...

 

http://www.generalpolymers.com/drop/3425E.pdf

 

Thanks!

 

Steve Gregory

Process Engineer

Kimco Design and Manufacturing

652 N. Five Mile Road

Boise, ID 83713

(208) 322-0500 Ext. 3133

 


______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________


______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

ATOM RSS1 RSS2