TECHNET Archives

January 1997

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Received:
by ipc.org (Smail3.1.28.1 #2) id m0vkv1Q-0000SHC; Thu, 16 Jan 97 10:50 CST
Old-Return-Path:
Date:
Thu, 16 Jan 97 08:24:14
Precedence:
list
Resent-From:
Resent-Sender:
TechNet-request [log in to unmask]
X-Status:
Status:
O
X-Mailing-List:
<[log in to unmask]> archive/latest/9301
TO:
Return-Path:
<TechNet-request>
Resent-Message-ID:
<"PXmwN.0.PML.Rnbto"@ipc>
From [log in to unmask] Thu Jan 16 11:
05:08 1997
From:
"Lynch, Lyn" <[log in to unmask]>
Subject:
X-Loop:
Message-Id:
Parts/Attachments:
text/plain (39 lines)

     Bill,
     
     Someone has already suggested ionizing air streams for reducing 
     electrostatic charges during mask and demask.
     
     I assume that the operator, spray booth, workpiece support and spray 
     gun nozzle are all at ground potential. Of course, the circuit itself 
     must also be at this potential. 
     
     For ultimate protection, I'd also attach a shorting bar across all
     connector fingers and tie that to your ground buss. Remember, all 
     those tiny blobs of conformal coating are non conductive.
     
     I also assume that your earth ground is totally isolated from
     all electrical feeds and prepared in such a way as to be effective 
     in all climatic conditions.(such as very dry) There is a Mil Spec on 
     earth grounding stations. This information was all gathered in another 
     life, so I don't remember the specific specification.
     
     The opinions stated herein are not those of my employer.
     
     
     Lyn R. Lynch
     602.276.7361
     

***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To unsubscribe from this list at any time, send a message to:           *
* [log in to unmask] with <subject: unsubscribe> and no text.        *
***************************************************************************
* If you are having a problem with the IPC TechNet forum please contact   *
* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask]      *
***************************************************************************



ATOM RSS1 RSS2