TECHNET Archives

April 1997

TechNet@IPC.ORG

Options: Use Monospaced Font
Show HTML Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Received:
by ipc.org (Smail3.1.28.1 #2) id m0wLwdl-000BjMC; Mon, 28 Apr 97 15:03 CDT
Encoding:
41 Text
From [log in to unmask] Tue Apr 29 10:
42:08 1997
Old-Return-Path:
Date:
Mon, 28 Apr 97 15:07:02 PST8
Precedence:
list
Resent-From:
Resent-Sender:
TechNet-request [log in to unmask]
X-Status:
Status:
O
X-Mailing-List:
<[log in to unmask]> archive/latest/12289
TO:
Return-Path:
<TechNet-request>
Resent-Message-ID:
<"c6gJq2.0.K19.-9GPp"@ipc>
Subject:
From:
X-Loop:
Message-Id:
Parts/Attachments:
text/plain (54 lines)
     

     Bob
     
        Common sense :-)  Fit, Function, and Reliability should be your 
     guidance. Insure that the wire will not snag or break from stress and 
     material fatigue during normal handling and use in the product. 
     Support within 1 inch of the connection, to strain relief the solder 
     joint, is a good minimum to start with.
     
     
______________________________ Reply Separator _________________________________
Subject: assembly-jumper wires
Author:  [log in to unmask] at CCGATE
Date:    4/28/97 11:21 AM
     
     
  To whom...                                                    28 Apr 97
     
     If I have wire jumpers on a mulitlayer pwb, is there a standard that
  defines the distance between bond points on the wire length. I know that 
  Mil-Std-275 and IPC-2221 both call out bonding at 1" intervals, but I am 
  looking at test set equipement, not hi-rel avionics hardware and IMO
  the 1" interval is an overkill. Is there any guidence, good commercial 
  standard, out there or if not, what is being done?  Thanks in advance.
     
                                                Regards,
  Bob Vanech                                              Bob 
  Norden Systems
  (203) 852-4810   
     
*************************************************************************** 
* TechNet mail list is provided as a service by IPC using SmartList v3.05 * 
*************************************************************************** 
* To subscribe/unsubscribe send a message <to: [log in to unmask]>   * 
* with <subject: subscribe/unsubscribe> and no text in the body.          * 
*************************************************************************** 
* If you are having a problem with the IPC TechNet forum please contact   * 
* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask]      * 
***************************************************************************
     

***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To subscribe/unsubscribe send a message <to: [log in to unmask]>   *
* with <subject: subscribe/unsubscribe> and no text in the body.          *
***************************************************************************
* If you are having a problem with the IPC TechNet forum please contact   *
* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask]      *
***************************************************************************



ATOM RSS1 RSS2