TECHNET Archives

October 2016

TechNet@IPC.ORG

Options: Use Proportional Font
Show HTML Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
"Stadem, Richard D." <[log in to unmask]>
Reply To:
TechNet E-Mail Forum <[log in to unmask]>, Stadem, Richard D.
Date:
Tue, 18 Oct 2016 14:06:05 +0000
Content-Type:
text/plain
Parts/Attachments:
text/plain (44 lines)
Ditto, XRF

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Fox, Ian
Sent: Tuesday, October 18, 2016 8:41 AM
To: [log in to unmask]
Subject: Re: [TN] Measuring Gold Thickness

Ditto

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Bev Christian
Sent: 18 October 2016 14:38
To: [log in to unmask]
Subject: Re: [TN] Measuring Gold Thickness

XRF

Bev

Sent from my BlackBerry 10 smartphone on the Bell network.
  Original Message
From: Bob Wettermann
Sent: Tuesday, October 18, 2016 9:28 AM
To: [log in to unmask]
Reply To: TechNet E-Mail Forum
Subject: [TN] Measuring Gold Thickness

Outside of x-sectional measurements for QA. can someone please share their favorite method/instrument for measuring gold thicknesses on PCBs?

Thanks

Bob/BEST
The data contained in, or attached to, this e-mail, may contain confidential information. If you have received it in error you should notify the sender immediately by reply e-mail, delete the message from your system and contact +44 (0) 3301235850 (Security Operations Centre) if you need assistance. Please do not copy it for any purpose, or disclose its contents to any other person.

An e-mail response to this address may be subject to interception or monitoring for operational reasons or for lawful business practices.

(c) 2016 Rolls-Royce plc

Registered office: 62 Buckingham Gate, London SW1E 6AT Company number: 1003142. Registered in England.

______________________________________________________________________
This email has been scanned.

ATOM RSS1 RSS2