I was wondering if any of you fabricators out there would provide me
with information on the following:

a.  method of regerating CuCl2 final etch with sodium chlorate,
including sodium chlorate concentration, HCl additions, rate of
additions, equipment used;

b.  method of automated control (ie. ORP control versus colormetric
control); and

c.  opinions on the ease of use (or lack thereof) of sodium chlorate
versus chlorine gas;

Thanks for you help!

Ted Stern
612-479-6525
[log in to unmask]

***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To unsubscribe from this list at any time, send a message to:           *
* [log in to unmask] with <subject: unsubscribe> and no text.        *
***************************************************************************
* If you are having a problem with the IPC TechNet forum please contact   *
* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask]      *
***************************************************************************



ATOM RSS1 RSS2