TECHNET Archives

October 1999

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
"Tempea, Ioan" <[log in to unmask]>
Date:
Mon, 4 Oct 1999 16:18:48 -0500
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, pod <[log in to unmask]>
Subject:
MIME-Version:
1.0
Content-Transfer-Encoding:
7bit
Content-Type:
text/plain; charset="iso-8859-1"
From:
Parts/Attachments:
text/plain (95 lines)
How inane, but what's changed? What processes as solder or flux composition,
or board configurations, or handling, or plating, or maintenance, or
calibration - have changed? If it worked before, didn't it, what is
different in the process.

Of course, the board thickness and thermal mass is "impossible" but it
worked before, right? How well did it really?

Earl Moon
----- Original Message -----
From: Tempea, Ioan <[log in to unmask]>
To: <[log in to unmask]>
Sent: Monday, October 04, 1999 3:45 PM
Subject: [TN] Cold solder


> Hi Technos,
>
> I'm in big trouble with a backplane.
>
> It's a 13.5"x19.5", 3.7mm thick. The connectors are disposed in parallel
> lines, forming two columns a the two extremities. In the middle we have no
> components. In between the connectors there are some TH caps and
resistors.
>
> ______________________________
> ______                                ______  I
> ______                                ______  I
> ______                                ______  I
> ______                                ______  I
> ..                                          ..
> ..
> ______                                ______  I
> _______________________________ I
>
> For a long time the soldering was OK, with small problems in the four
> corners ( a couple of holes not 100% full).
>
> For about a week or so, the solder joints of many caps or resistors
present
> cold solder. There are no significant cold solder problems with the
> connectors, which present though a little less wetting (some of the
fillets
> are not what they used to be).
>
> The question is: why do I get the cold solder and how can I get read of
it?
>
> We use :
> - no-clean technology
> - Multicore Sn63 solder
> - Multicore X33 flux
> - strong radiation preheating ( two top preheaters at 700F and two bottom
at
> 750F); we spent a lot of time tweaking to avoid damaging the board
> - two passes, one for fluxing only, no wave, the second one right after
with
> no fluxing, but with wave
> - no chip wave (that's what I have, hehehe), just omega on our Electrovert
> Econopak II
>
> Any help would be greatly appreciated.
>
> Thanks,      Ioan
>
> ##############################################################
> TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
> ##############################################################
> To subscribe/unsubscribe, send a message to [log in to unmask] with
following text in
> the body:
> To subscribe:   SUBSCRIBE TECHNET <your full name>
> To unsubscribe:   SIGNOFF TECHNET
> ##############################################################
> Please visit IPC web site (http://www.ipc.org/html/forum.htm) for
additional
> information.
> If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
> 847-509-9700 ext.5365
> ##############################################################

##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe:   SUBSCRIBE TECHNET <your full name>
To unsubscribe:   SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
847-509-9700 ext.5365
##############################################################

ATOM RSS1 RSS2