Hi ya'll...
Well I've run into a problem again that I've experienced a few times before.
I've got a board (actually 3 boards) here, where the solder mask has come off
all the surface traces. I know what's caused it, it's because of a certain
brand dry-film mask is not compatible with the brand of cleaning chemistry
that we use, the mask starts flaking off if it's washed more than twice I
don't want to mention names because I upset some people last time when I
did...
The problem is how can I go about repairing the boards. It's a small
double-sided board with some very long lead time PTH resistors on it and
2-connectors, and as I said, it's only 3-boards.
The board is hi-rel, and these 3 boards are needed to complete a system. The
board gets conformal coated as a normal part of the process. We spray a
2-part urethane here, but at one of our other facilities we do have paralene
vapor deposition capabilities.
I know trying to touch-up the mask is out of the question because as I said,
the mask has flaked-off of all the surface traces. Do any of you have a
opinion as to whether the urethane would be sufficient, or should I use
paralene? I tend to think that paralene would be better because of it's
strength and ability to coat all surfaces well.
-Steve Gregory-
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
##############################################################
|
|
|