TECHNET Archives

September 2006

TechNet@IPC.ORG

Options: Use Monospaced Font
Show HTML Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, "Ingemar Hernefjord (KC/EMW)" <[log in to unmask]>
Date:
Thu, 14 Sep 2006 10:12:19 -0400
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Joe Russeau <[log in to unmask]>
Subject:
MIME-Version:
1.0
Content-Transfer-Encoding:
7bit
Content-Type:
text/plain; charset="iso-8859-1"
From:
Joe Russeau <[log in to unmask]>
Parts/Attachments:
text/plain (105 lines)
Hi Inge,

I would be interested in the table.  Oh, and thank you for making the offer!

Best Regards,

Joe Russeau
Process Analyst

Precision Analytical Laboratory, Inc.
4106 Cartwright Dr. Ste. A
Kokomo, IN 46902

P: 765-455-1993
F: 765-455-1996
E: [log in to unmask]


----- Original Message -----
From: "Ingemar Hernefjord (KC/EMW)" <[log in to unmask]>
To: <[log in to unmask]>
Sent: Thursday, September 14, 2006 6:37 AM
Subject: Re: [TN] US Cleaning in IPA


> Furthermore, I have some values about the cavitation vs. Liquids vs.
> Temperature e.g. Below:
>
>
> Liquid          Formula         Boiling         Max cavitation intensity
> Temperature at which
>                                                                 for 46
> MHz lambda/2            reaches intensity max
>
> 1. Water                H2O             100 C
> 100%                                    35 C
>
> 2. Xylen                C6H4 etc        137 C
> 61%                                     93 C
>
> 3. Ethanol              C2H5OH  78  C                           45%
> 21 C
>
> 4. Aceton               (CH3)2CO        56  C
> 44%                             minus 36 C
>
> Etc
>
> Can send whole table to interested, or for Steve's wall
>
>
> Inge
>
> -----Original Message-----
> From: TechNet [mailto:[log in to unmask]] On Behalf Of [log in to unmask]
> Sent: den 13 september 2006 20:51
> To: [log in to unmask]
> Subject: Re: [TN] US Cleaning in IPA
>
> 40 MHz was the typical frequency used for augmenting solvent cleaning.
> There is a classic paper by Brandreth & Johnson on removal of a
> standardized particle (diamond dust) published in 1978 as I recall. Will
> send you the exact reference later if you are interested-- let me know.
> 25-28 MHz was more typically used with aqueous systems until we got into
> the more elaborate multi-frequency systems.
>
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
> unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
> (re-start) delivery of Technet send e-mail to [log in to unmask]: SET
> Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
> posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
> archives of previous posts at: http://listserv.ipc.org/archives Please
> visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
> additional information, or contact Keach Sasamori at [log in to unmask] or
> 847-615-7100 ext.2815
> -----------------------------------------------------
>
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 1.8e
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
> Search the archives of previous posts at: http://listserv.ipc.org/archives
> Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
> -----------------------------------------------------
>
>

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2