TECHNET Archives

November 1997

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Content-Transfer-Encoding:
7bit
Sender:
Subject:
From:
Date:
Thu, 20 Nov 1997 20:56:11 -0800
Content-Type:
text/plain; charset=us-ascii
MIME-Version:
1.0
Reply-To:
Parts/Attachments:
text/plain (42 lines)
Can anyone shed any light on the cause and cure of the following problem?
Some test panels with edge connectors were gold plated on a tab plater:-

        Electropolish - phosphoric acid
        rinse
        activate - 10% sulphuric acid
        rinse
        gold plate - nickel hardener
        rinse
        dry

These boards were then passed through a conveyorized solder resist curing oven.

The area  exposed to the tab plater solution turned a red/ purple colour.

Other boards also tab plated were washed in a post hasl cleaner, passed through a 3%
caustic soda coveyorized resist stripper and finally passed through a brushing machine.

When passed through the the resist curing oven the area exposed to the tab plater
solutions turned red/purple.

When I tested the insulation resistance between the edge connector fingers on the
stained boards at 1000 volts it was 145 gigohms.

Some of the stain can be removed with acetone but not other solvents.

Thankyou in advance

Roger Hammond

##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe:   SUBSCRIBE TECHNET <your full name>
To unsubscribe:   SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional information.
For the technical support contact Dmitriy Sklyar at [log in to unmask] or 847-509-9700 ext.311
##############################################################


ATOM RSS1 RSS2