Yes Sn96 has been used for decades as a higher temp alternative to Sn63/Sn62
especially in hybrid thick film apps.
The addition of Cu does drop melting temperature 4C from 221 to a notional
217C, the addition also improves the alloy properties of the solder as a
solder and in life cycling. Joint properties on ENIG are subject to the same
problems as SAC. 





Regards 

Mike Fenner 
Indium Corporation 

T: + 44 1908 580 400 
M: + 44 7810 526 317 
F: + 44 1908 580 411 
E: [log in to unmask] 
W: www.indium.com 
Pb-free: www.Pb-Free.com 



-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Macconnell, Richard (ES)
Sent: Friday, September 22, 2006 4:32 PM
To: [log in to unmask]
Subject: Re: [TN] Soldering with Sn9,5Ag3,5

Arnaud:

We use Sn96 (referred to as high-temp solder) in processes where there are
two soldering operations.  Sn63 solder is used in the first operation,
followed by the Sn96 in the second.  This avoids reflowing the Sn63 during
the second soldering.

I don't know enough about soldering to be able to answer Juan's question.
But, if the intent is to solder the tinned wires to the board, isn't some
melting of the SnPb coating on the board required?  If so, why use a
high-temp solder?  Switching to ENIG gets around that issue.

Rich. 

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of arnaud grivon
Sent: Friday, September 22, 2006 6:20 AM
To: [log in to unmask]
Subject: Re: [TN] Soldering with Sn9,5Ag3,5

Could anybody on the TechNet planet tell me the primarily reasons for using
this Sn96,5Ag3,5 solder alloy?
It looks like this alloy has been already in use for some years as solder
wires and solder paste for small electronic modules.
Also, I seem to remind that this was the first alloy of choice for lead-free
BGA spheres before the industry consensus for SAC.
Why did the industry switch to SAC instead of SnAg? In other words, what
does the copper bring?

A. Grivon

Juan T. Marugán a écrit :
> Hi,
>
> in a Class 3 product (aerospace) we have to solder some wires to a PCB 
> using a Sn96,5Ag3,5 solder alloy. Wires are silver coated, 
> high-strength copper alloy and the PCB is SnPb plated.
>
> My first question is, Do you consider that solder alloy as a good option?
>
> Besides, in a near future, we will change the finish of the PCB from 
> SnPb to ENIG. In that situation, what solder alloy do you recommend us?
>
> Thank you in advance.
>
> Juan T. Marugán
> Production QA
> Indra Sistemas SA
> Spain
>
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 1.8e To 
> unsubscribe, send a message to [log in to unmask] with following text in 
> the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt 
> or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET 
> Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the 
> posts: send e-mail to [log in to unmask]: SET Technet Digest Search the 
> archives of previous posts at: http://listserv.ipc.org/archives Please 
> visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 
> for additional information, or contact Keach Sasamori at 
> [log in to unmask] or 847-615-7100 ext.2815
> -----------------------------------------------------
>   

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
unsubscribe, send a message to [log in to unmask] with following text in the
BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet
NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send
e-mail to [log in to unmask]: SET Technet Digest Search the archives of
previous posts at: http://listserv.ipc.org/archives Please visit IPC web
site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------


***This email, its content and any files transmitted with it are intended solely for the addressee(s) and may be legally privileged and/or confidential. If you are not the intended recipient please delete and contact the sender by return and delete the material from any computer. Any review, retransmission, dissemination or other use of, or taking of any action in reliance upon, this information by persons or entities other than the intended recipient is prohibited. 

Messages sent via this medium may be subject to delays, non-delivery and unauthorized alteration. This email has been prepared using information believed by the author to be reliable and accurate, but Indium Corporation makes no warranty as to accuracy or completeness. In particular, Indium Corporation does not accept responsibility for changes made to this email after it was sent. Any opinions or recommendations expressed herein are solely those of the author. They may be subject to change without notice.***

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2