Bill

you wrote
>We have had numerous experiences where the component package was only
available in LCC format but we needed to use the component in a military
application where vibration testing and thermal testing is done. We take the
LCC packaged component and ship them to North Penn Technology in Hatfield,
PA where they attach "J" leads to the LCC.<

Can you mail me the address of North Penn Technology?
Thank you

Best regards

Guenter


***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To subscribe/unsubscribe send a message <to: [log in to unmask]>   *
* with <subject: subscribe/unsubscribe> and no text in the body.          *
***************************************************************************
* If you are having a problem with the IPC TechNet forum please contact   *
* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask]      *
***************************************************************************


ATOM RSS1 RSS2