Hello, Kuan,
Why don't you try Kyocera, Sumitomo, NTK or other japanese
manufacturers. They are probably the world's best on ceramics for large
series.
                             //Ingemar

> Hi,
>
> I hope someone can help me out on this. I am looking for substrate
> manufacturers who make LTCCs with buried capacitors and resistors. I
hope
> they also support prototyping work. To date we have written to
companies
> such as Scrantom Engineering, Maxtek Corp, Automata but have not
receive
> any replies from them. Perhaps we don't meet their customer selection
> criterion.
>
> I hope you can help me out on this. I thank you all in advance.
>
> Rgds - Kuan
>
>
>
> Kuan Kuan Ng
> DSO National Laboratories
> 20 Science Park Drive
> Singapore 118230
> Voice: (65) 772-7126
> Fax: (65) 775-9011
> E-mail: [log in to unmask]
>
> ################################################################
> TechNet E-Mail Forum provided as a free service by IPC using LISTSERV
1.8c
> ################################################################
> To subscribe/unsubscribe, send a message to [log in to unmask] with
following text
>  in the body:
> To subscribe:   SUBSCRIBE TechNet <your full name>
> To unsubscribe:   SIGNOFF TechNet
> ################################################################
> Please visit IPC's web site (http://www.ipc.org) "On-Line Services"
section for
> additional information.
> For technical support contact Hugo Scaramuzza at [log in to unmask] or
847-509-9700
> ext.312
> ################################################################
>

################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe:   SUBSCRIBE TechNet <your full name>
To unsubscribe:   SIGNOFF TechNet 
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################


ATOM RSS1 RSS2