TECHNET Archives

January 1997

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Received:
by ipc.org (Smail3.1.28.1 #2) id m0vkwLE-0000QBC; Thu, 16 Jan 97 12:15 CST
Content-Type:
text/plain; charset=us-ascii
CC:
References:
Date:
Thu, 16 Jan 1997 11:35:02 -0800
Precedence:
list
Resent-From:
Resent-Sender:
TechNet-request [log in to unmask]
MIME-Version:
1.0
Status:
O
X-Mailing-List:
<[log in to unmask]> archive/latest/9306
From [log in to unmask] Thu Jan 16 15:
11:48 1997
TO:
sam mccorkel <[log in to unmask]>
Return-Path:
<TechNet-request>
X-Status:
X-Loop:
Content-Transfer-Encoding:
7bit
Resent-Message-ID:
<"mFxDG1.0.YRG.h0dto"@ipc>
Subject:
From:
Pratap Singh <[log in to unmask]>
Old-Return-Path:
Message-ID:
Organization:
RAMP Inc
X-Mailer:
Mozilla 2.01KIT (Win16; U)
Parts/Attachments:
text/plain (43 lines)
sam mccorkel wrote:
> 
> I'm looking for any cautions or advice you may have on the following.
> We are considering the use of immersion tin as a finish on bare printed
> circuit boards.
> The boards are thru-hole only and they will be wave soldered within the next
> 3-4 weeks.
> Do you consider this a "no no" or is this an acceptable finish until wave
> soldering?
> 
> ***************************************************************************
> * TechNet mail list is provided as a service by IPC using SmartList v3.05 *
> ***************************************************************************
> * To unsubscribe from this list at any time, send a message to:           *
> * [log in to unmask] with <subject: unsubscribe> and no text.        *
> ***************************************************************************
> * If you are having a problem with the IPC TechNet forum please contact   *
> * Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask]      *
> ***************************************************************************
Do not use TIN coatings on PCB. Have you not read about Tin-Whisker 
growth on tin coated boards that cause random short failures.

This mechanism has ben documented in several papers. Recently, a few 
emails have beeen posted about the same mechanism. 


-- 
Pratap Singh
Tel./Fax: 512-255-6820
e-mail: [log in to unmask]

***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To unsubscribe from this list at any time, send a message to:           *
* [log in to unmask] with <subject: unsubscribe> and no text.        *
***************************************************************************
* If you are having a problem with the IPC TechNet forum please contact   *
* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask]      *
***************************************************************************



ATOM RSS1 RSS2