TECHNET Archives

September 1997

TechNet@IPC.ORG

Options: Use Proportional Font
Show HTML Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
David D Hillman <[log in to unmask]>
Reply To:
TechNet Mail Forum.
Date:
Thu, 18 Sep 1997 07:18:18 -0500
Content-Type:
text/plain
Parts/Attachments:
text/plain (69 lines)
Hi Stein -
There are a number of water soluble, acid fluxes that you could use for
your tinning operation for several manufacturers. I have seen the Superior
30 work well in several applications. I am surprised that the ESA
specification (this is one spec I have never seen) allows the use of a acid
flux in place of a RMA, especially for space applications. Whatever acid
flux you do choose I would suggest you run some cleanliness tests to assure
yourself that your tinning process does not leave a  residue on the
components that could lead to corrosion. Good Luck.


Dave Hillman
Rockwell Collins
[log in to unmask]




[log in to unmask] on 09/17/97 06:50:40 AM

Please respond to [log in to unmask]; Please respond to
      [log in to unmask]

To:   [log in to unmask]
cc:    (bcc: David D Hillman/CedarRapids/Collins/Rockwell)
Subject:  [TECHNET] Pretinning - Flux




     Technetters,
     I have some problems pretinning some components stored for 5 years.
     The components shall be used in space equipment and according to
     ESA-PSS-01-708 we can use rosin based flux (RMA) for pretinning. If
     RMA flux are inadequate, corrosive water-soluble acid flux can be
     used.
     For our components RMA flux does not do the trick.
     1) Does anyone know a good method that can be used?
     2) Does anyone know suppliers of corrosive water-soluble acid fluxes?
     3) We have heard of a flux type called SUPERIOR 30. Can anyone tell me
        about suppliers of this flux?
     Thanks,
     Stein Davidsen
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following
text in the body:
To subscribe:   SUBSCRIBE TECHNET <your full name>
To unsubscribe:   SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for
additional information.
For the technical support contact Dmitriy Sklyar at [log in to unmask] or
847-509-9700 ext.311
##############################################################

##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe:   SUBSCRIBE TECHNET <your full name>
To unsubscribe:   SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional information.
For the technical support contact Dmitriy Sklyar at [log in to unmask] or 847-509-9700 ext.311
##############################################################


ATOM RSS1 RSS2