TECHNET Archives

July 2008

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Mime-Version:
1.0
Sender:
X-To:
Date:
Mon, 21 Jul 2008 08:58:20 -0500
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Pete Houwen <[log in to unmask]>
Subject:
Content-Transfer-Encoding:
quoted-printable
Content-Type:
text/plain; charset="windows-1252"
From:
Pete Houwen <[log in to unmask]>
Parts/Attachments:
text/plain (22 lines)
Our purchasing group is trying to qualify a new low cost PCB vendor, and I 
have some reservations.  I have been examining their sample boards, and while 
one oif them shows a normal ENiG grain under 800x magnification, the other is 
flat and dull.  I believe it might be just gold plating.  It's hard to tell from the 
cross sectons they sent (those display their own set of concerns).  I'm trying 
to find some images to compare these, but I'm having no luck.  Does anyone 
know of a good site where I might find some ENiG and Gold images?

Thanks,

Pete

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2