You have roused my curiosity, Phil. What are the parts that can
withstand halide-free WS fluxes but not halide-containing ones, and why?
I could understand it for some chemical sensors but optical??? Have you
discussed this with your parts manufacturer? Does he give a reason for
eschewing halides or is it aqueous processes that he does not like? What
is his view on halide-containing rosin fluxes?
Please let me warn you that you would need to re-qualify your process
because you may find that the halide-free fluxes may be a lot more
difficult to clean, especially with a DI-water only wash. You may find
that there may be more corrosive residues on the washed boards.
For me, assuming that my thoughts are justified, using your current
process with one small modification, perhaps not requiring
re-qualification, will fill the bill. That is to have a static bath
containing a chelating neutraliser (not a saponifier) between the
soldering and cleaning operations. A couple of minutes or so will
solubilise any heavy metal halides or organic halides and will "kill"
the excess acidity of any WS flux. I used to recommend Lonco 2051-B-3
but I think this is no longer available. I think Alpha have one called
Rinse-Aid and I suppose Kester, Multicore etc. may have equivalents.
Have you thought that many components are supplied with halides galore?
Component manufacturers often use halide fluxes for tinning their
products, often with little or even no cleaning. Much tinned copper wire
uses a zinc chloride/hydrochloric acid flux and the only cleaning is
running it through a damp sponge followed by a sponge with a waxy substance!
If your components are really sensitive to halide ions, I would say that
ion chromatography will be an essential part of your qualification
process, no matter which flux you use.
Finally, have you thought about using your existing process but adding
the sensitive components by hand, soldering with an evaporative
halide-free no-clean flux, after cleaning? this may a simple cheap way
round your problem, especially if the quantities are small.
Brian
PS Inge: Thanks for the plug. The IPC were kind enough to allow me to
mention the availability of the book on this forum a few months ago but
I don't want to abuse their hospitality, other than to say there is now
a download version as well as the hard copy. I'm now the publisher as
well as the author!
On 28/02/2012 21:12, Phil Nutting wrote:
> We have some parts that are sensitive to halides in flux, specifically some thru-hole opto devices. We are currently using a water soluble flux that contains halides. In doing some very quick research it looks like the WS fluxes have halides and the NC fluxes do not.
>
> Is there a halide free WS flux for lead-free wave soldering (foam application)?
>
> We need the WS fluxes because we currently use a DI water only batch wash system. Washing the boards is mandatory for our applications.
>
> Thanks in advance,
>
> Phil Nutting
> Design for Manufacturing Engineer
> Kaiser Systems, Inc.
> 126 Sohier Road
> Beverly, MA 01915
> Phone: 978-922-9300 x1310
> Fax: 978-922-8374
> e-mail: [log in to unmask]<mailto:[log in to unmask]>
> www.kaisersystems.com<http://www.kaisersystems.com>
> www.linkedin.com/in/philnutting<http://www.linkedin.com/in/philnutting>
>
>
> ________________________________
> Note: All the information contained in this e-mail and its attachments is proprietary to Kaiser Systems, Inc. and it may not be reproduced without the prior written permission of sender. If you have received this email in error, please immediately return it to sender and delete the copy you received.
>
>
> ______________________________________________________________________
> This email has been scanned by the Symantec Email Security.cloud service.
> For more information please contact helpdesk at x2960 or [log in to unmask]
> ______________________________________________________________________
>
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
|