TECHNET Archives

July 2000

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
"Hiteshew, Michael" <[log in to unmask]>
Date:
Wed, 12 Jul 2000 13:53:46 -0400
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, Bob Dube <[log in to unmask]>
Subject:
MIME-Version:
1.0
Content-Transfer-Encoding:
7bit
Content-Type:
text/plain; charset="iso-8859-1"
From:
Bob Dube <[log in to unmask]>
Parts/Attachments:
text/plain (67 lines)
1. Sort of. (from brittle to "rubbery", never really becomes a liquid before
decomposing)

2. Higher operating temp.

3. Yes.

Bob Dube

-----Original Message-----
From: Hiteshew, Michael <[log in to unmask]>
To: [log in to unmask] <[log in to unmask]>
Date: Wednesday, July 12, 2000 12:11 PM
Subject: [TN] Glass Transition Temperature (Tg) Questions


Hi,
        I've been reading up on laminate materials and have some questions
that I hope some-one can help me with:

1. What is the "glass transition" ? What is the glass transitioning from and
to? I'm guessing it's the plastic stage that occurs in a material just
before it melts.

2. What is gained by a higher Tg in tetrafunctional and multifunctional
epoxy-glass?

3. What is meant by the prefixes "tetra" and "multi" as they're applied
here? Is it a reference to the number on bonds in the chemical structure of
the epoxy or glass?

Thanks in advance,

Michael Hiteshew
Lockheed Martin NE&SS-Baltimore
[log in to unmask]
(410) 682-1259

##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following
text in
the body:
To subscribe:   SUBSCRIBE TECHNET <your full name>
To unsubscribe:   SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
##############################################################

##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe:   SUBSCRIBE TECHNET <your full name>
To unsubscribe:   SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
##############################################################

ATOM RSS1 RSS2