TECHNET Archives

January 2005

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, "Crepeau, Phil (Space Technology)" <[log in to unmask]>
Date:
Wed, 12 Jan 2005 12:52:17 -0500
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Lee Parker <[log in to unmask]>
Content-Transfer-Encoding:
7bit
Subject:
From:
Lee Parker <[log in to unmask]>
Content-Type:
text/plain; charset="us-ascii"
In-Reply-To:
MIME-Version:
1.0
Comments:
RFC822 error: <W> MESSAGE-ID field duplicated. Last occurrence was retained.
Parts/Attachments:
text/plain (145 lines)
I like that!!

In my home state of North Carolina there is an excellent school of
engineering called NC State University, there is also a private
want-to-be located a few miles to the west on the wrong side of RTP. The
most enlighten want-to-be's usually go on to grad school at NCS where
they are gently oriented into the world of real engineering. I am sure
those who successfully completed this orientation will agree.

My point being is that the accomplishments of state supported schools is
incredible!

Lee

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Crepeau, Phil (Space
Technology)
Sent: Wednesday, January 12, 2005 11:19 AM
To: [log in to unmask]
Subject: Re: [TN]

hi,

my school (public) has a major, natural rival (private).  when asked by
alumni and fans of the private school why we'd ever want to go the a
lowly public school, our reply would be, 'i'd rather earn my degree than
buy it'.

phil

-----Original Message-----
From: TechNet [mailto:[log in to unmask]]On Behalf Of Jeffrey Bush
Sent: Wednesday, January 12, 2005 7:43 AM
To: [log in to unmask]
Subject: Re: [TN]


Like an education, the best place to buy boards is on the East Coast.

Jeffrey Bush
Director, Quality Assurance and Technical Support

VERMONT CIRCUITS INCORPORATED
  76 Technology Drive - POB 1890
    Brattleboro, Vermont 05302
      Voice: 802.257.4571.21 Fax: 802.257.0011
           http://www.vtcircuits.com


-----Original Message-----
From: Gary Bremer [mailto:[log in to unmask]]
Sent: Wednesday, January 12, 2005 10:18 AM
To: [log in to unmask]
Subject: [TN]

Hello Designer Council members

At the company I am working for is calling out matterial .062 thick FR4
green
copperclad laminate for their bare board.

My question for the form:

When this design was done in the Northeast by the electrical engineer
and
outsourced to a board assembly house as a turnkey component.  What type
of
quality problems can I expect to deal with durning final assembly and
final
test?  What long term (customer returns) problems may result from this?
Do the
board fabracation houses on the east coast march to a different drummer
than
the rest of the country?  The electrical engineer does not want to
change the
drawing to specify what laminate matterial he truly intends to use.  The
last
company I worked for also had this same type of problem.  The electrical
engineer designs/releases and I have to fix his mistakes.

Gary Bremer
Senior Manufacturing Engineer
Company located in California

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2