TECHNET Archives

March 1997

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Received:
by ipc.org (Smail3.1.28.1 #2) id m0w1ZE0-0007zXC; Mon, 3 Mar 97 09:00 CST
Content-Type:
text/plain; charset="iso-8859-1"
Old-Return-Path:
Date:
Mon, 3 Mar 1997 09:19:37 -0600
Precedence:
list
Resent-From:
Resent-Sender:
TechNet-request [log in to unmask]
MIME-Version:
1.0
Status:
O
X-Mailing-List:
<[log in to unmask]> archive/latest/10792
TO:
"'peer fisker'" <[log in to unmask]>
Return-Path:
<TechNet-request>
X-Status:
X-Loop:
Resent-Message-ID:
<"TJHWS1.0.RVE.7Uk6p"@ipc>
Subject:
From:
Ed Cosper <[log in to unmask]>
From [log in to unmask] Tue Mar 4 08:
41:59 1997
Content-Transfer-Encoding:
quoted-printable
Message-ID:
<01BC27B4.092D6DE0@gateway>
Cc:
Parts/Attachments:
text/plain (56 lines)
I have found the best surface prep for innerlayers is a combination of a pre-dip microetch followed by an aluminum oxide scrub. The microetch (we use an SP) provides a roughened surface conducive to adhesion of the resist without the potential scrub lines associated with mechanical scrubbing. The aluminum oxide provide a polish an leave the surface virtually free of oxidation without smoothing out the topography created by the microetch. We have also found a final DI rinse slightly acidic provides better adhesion.  

Hope this helps,

Ed Cosper
Director, Quality Assurance and Engineering
Graphic Electronics Inc.

----------
From:  peer fisker[SMTP:[log in to unmask]]
Sent:  Monday, March 03, 1997 9:19 AM
To:  [log in to unmask]
Subject:  fab

subject: pretreatment of innerlayers

to improve yields in innerlayers production, we are considering the use 
of chemical cleanning instead of pumicebrush prior to lamination of 
photoresist.
there is a new trend towards using chemical cleaning only to remove 
passivation (e.g. chromate) and impurities like organics, oxides etc.
this should be achieved by a hot alkaline spray cleaner followed by a 
ordinary acidic spray cleaner.
we are using FR4-copperclad, thickness 0,10 to 0,70 mm, copperfoil; 12 
to 70 µm. the thickness of the passivationlayer is 7,0 nm (0,007 µm).

If you have had used/or are using this new principle of pretreatment of 
innerlayers, we would like to hear what was/ is your experience with the 
process. 

best regards 
peer fisker

***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To subscribe/unsubscribe send a message <to: [log in to unmask]>   *
* with <subject: subscribe/unsubscribe> and no text in the body.          *
***************************************************************************
* If you are having a problem with the IPC TechNet forum please contact   *
* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask]      *
***************************************************************************


***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To subscribe/unsubscribe send a message <to: [log in to unmask]>   *
* with <subject: subscribe/unsubscribe> and no text in the body.          *
***************************************************************************
* If you are having a problem with the IPC TechNet forum please contact   *
* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask]      *
***************************************************************************



ATOM RSS1 RSS2