Hi Dan - I went through my files and found a couple of papers that might be
useful:
"The Rough or Grainy Solder Phenomenon", Ronald Bulwith, PC Fab October
1986, pp23-35.
"??? On Surface Mount Components", H. Steen, Circuit World, Vol. 112, No.
1, 1984,
(I lost the first title words due to a poor photocopy)
Most technologist would not want a cold solder joint (per IPC -T-50
definition) on an assembly because in most use environments the reliability
would be terrible. Good Luck.
Dave Hillman
Rockwell Collins
[log in to unmask]
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional information.
For the technical support contact Dmitriy Sklyar at [log in to unmask] or 847-509-9700 ext.311
##############################################################
|
|
|