TECHNET Archives

October 2011

TechNet@IPC.ORG

Options: Use Proportional Font
Show HTML Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
Karen Tellefsen <[log in to unmask]>
Reply To:
TechNet E-Mail Forum <[log in to unmask]>, Karen Tellefsen <[log in to unmask]>
Date:
Tue, 11 Oct 2011 08:52:22 -0400
Content-Type:
text/plain
Parts/Attachments:
text/plain (147 lines)
Ditto.  This flux is very corrosive.  From J-STD-004 H means high activity,
1 means with halide, Mumtaz provided more details.  This flux is designed
to be washed off.  If ANY moisture gets through the gasket, this circuit
will have problems.  Would it be possible to solder this one part with ROL1
or REL1 flux -cored solder wire and no assist flux?

Karen Tellefsen - Electrical Testing
[log in to unmask]
908-791-3069



                                                                            
                                                                            
                                                                            
   Re: [TN] ORH1 flux residues                                              
                                                                            
                                                                            
   Robert Kondner                                                           
                  to:                                                       
                    TechNet                                                 
                                                        10/10/2011 08:14 PM 
                                                                            
                                                                            
                                                                            
                                                                            
   Sent by:                                                                 
          TechNet <[log in to unmask]>                                         
   Please respond to rkondner                                               
                                                                            
                                                                            
                                                                            






I would suggest it is VERY bad thing.

 If that flux is an ionic material, and I think the H1 indicates it is,
then
you have a serious problem with everything you ever built using that
technique. That flux, remaining on a PCB, and in the presence of a voltage,
will grow all kinds of evil stuff.

 I hope someone can tell me wrong.

Bob K.

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Phil Bavaro
Sent: Monday, October 10, 2011 7:49 PM
To: [log in to unmask]
Subject: [TN] ORH1 flux residues

I have a PWA with a gasket beneath a large thru hole power device.
The gasket has holes punched in it for each of the pins.
The device is hand soldered flush to the PWB.
The operator uses external liquid flux along with core solder with flux in
it.
The assembly is later washed and it passes ionics testing.

The problem is that this gasket effectively seals the top side solder
connections from the cleaning process.


My question is this:

How much should I be worrying about the existing hardware which has flux
residues sealed under the power device?
The assembly is stored with the power off.
The flux used is water soluble and classified as ORH1.
For future builds we are modifying the gasket so that the topside
connections can be cleaned (cutout "u" shape intead of round holes).



----------------------------------------------------------------------------

--
This message and any attachments are solely for the use of the addressee
and
may contain L-3 proprietary information that may also be defined as USG
export controlled technical data. If you are not the intended recipient,
any
disclosure, use or distribution of its content is prohibited. Please notify
the sender by reply e-mail and immediately delete this message and any
attachments.




______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 16.0 To
unsubscribe, send a message to [log in to unmask] with following text in the
BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet
NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send
e-mail to [log in to unmask]: SET Technet Digest Search the archives of
previous posts at: http://listserv.ipc.org/archives For additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------


______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 16.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
For additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------




______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 16.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
For additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2