TECHNET Archives

November 2012

TechNet@IPC.ORG

Options: Use Monospaced Font
Show HTML Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
Date:
Wed, 14 Nov 2012 14:02:51 -0800
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, [log in to unmask]
Subject:
From:
John Burke <[log in to unmask]>
Message-ID:
In-Reply-To:
<34C0FC3245BB40F2AF036A39BE164FA3@MikePC>
Content-Type:
text/plain; charset="US-ASCII"
MIME-Version:
1.0
Parts/Attachments:
text/plain (102 lines)
Hi Amol how is life at AFG??

 I would advise that they use leaded solder (heh heh) reflow at lead free 
temperatures peaking at say 240C and use a flux that is rated for lead 
free soldering. Such a leaded/flux combination can be obtained from AIM 
WS-488 63/37 is the part number for the paste

Best regards


John Burke

General Manager/COO

Zollner Electronics Inc
Plant Milpitas
575 Cottonwood Drive
Milpitas, CA 95035
Phone:          + 1 408 434 5442
Fax:            + 1 408 434 5401
Mobile:         + 1 408 628 2433
E-mail:         [log in to unmask]
Internet:  www.zollner-electronics.com


-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Amol Kane
Sent: Tuesday, November 13, 2012 4:05 PM
To: [log in to unmask]
Subject: [TN] SnPb and Pb-free paste mixture

Hi,
We have this unusual (at least for me) request from a potential new
customer. This is taken verbatim from their request for process 
information.
Before I go and tell them this cannot be done, I want to ask the experts 
out
on technet if they have seen/done something like this. My thinking is that
this would be very hard to do on the floor unless there is a custom
formulation available. I am not aware of their reasoning for asking this
other than for a very unusual (and ineffective) way of mitigating tin
whiskers. Leaving the potential flux incompatibilities aside, is this
something that is being done/can be done? I could use some expertise or
references/studies on # 2 as well.


1.       "Since our products are not subject to RoHS and our customer is 
not
requiring lead mitigation, is there a vendor preferred process of Pb based
or Pb-free processing.

a.       Describe your history/experience and process for adding ~3% Pb to
Pb-free paste and utilizing Pb-free processes.

b.      Any quality or reliability concerns adding ~3% Pb to Pb-free
soldering.

c.       Describe your history/experience and processes used in
transitioning a product from Pb to Pb-free (or reduced Pb).

2.       Do you know of any issues with RoHS and reliability at -65C?"

Thanks,
Amol

________________________________
Confidentiality Notice

This e-mail and any attachment(s) are intended for the individual or 
entity
to which this email is addressed and may contain information that is
confidential. If you are not the intended recipient or an employee or 
agent
responsible for delivering this e-mail to the intended recipient, please 
be
aware that any dissemination, distribution or copying of this 
communication
is strictly prohibited. If you have received this in error, please notify
the sender by telephone at 604.430.4336 or by return e-mail, and please
delete or destroy all copies of this communication. Thank you!

P     Please consider the impact on the environment before printing this
email or its attachments

______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________



______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________


______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

ATOM RSS1 RSS2