Hi Jerry,
I prefer the via's to be closed on both sides, or open on both sides.
When only one side has soldermask you could see some problems from the HASL process, because the solder (and fluxes, and cleaning agents) can't flow very well through these holes. Not a good way to achieve a smooth and clean solder coating in these via's.
Kind regards,
Daan Terstegge
SMT Centre
Thales Communications
Unclassified mail
Personal Website: http://www.smtinfo.net
>>> Jerry Mosur <[log in to unmask]> 04/10 4:03 pm >>>
Hello,
Have anyone specified via solder mask on top and not on bottom? I am trying
to fill-in vias as much as I can. What pitfalls in term of assembly,
reliability, etc.. I can expect?
Thanks,
Jerry
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|