Hello Gregg.
If you disallow the individual strands to go where they need to go
during the crimping process, fractures will occur. Improper
displacement. We all want the best electrical connection we can get. IDC
has solidified (a pun) that statement.
Crimp a contact to a solid wire. Cross section it and tell me what you
see. Fractures within the solid wire. Nowhere for it to go.
Crimp a contact to a stranded wire. Cross section it and tell me what
you see. Proper displacement (as long as the contact and the wire are
within the gauges by design.)The strands are all in the cavities where
they need to be.
Bryon Boone
Technical Training Manager, CIT
Carlisle Interconnect Technologies
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Gregg Owens
Sent: Tuesday, May 31, 2011 10:24 AM
To: [log in to unmask]
Subject: [TN] Tinning Stranded Wire - Crimped Connections
Dear Technetters:
I have been posed a question I can't answer. In both the IPC-A-610 and
IPC-A-620 require that stranded wires used for crimp connections NOT be
pre-tinned with solder. Okay I get the requirement, but does anyone know
why this is a requirement. Pre-tinning keeps the strands together, so
there is some push-pack on why this is a requirement. Any thought
appreciated.
Gregg Owens
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or
[log in to unmask]
______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 16.0
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
For additional information, or contact Keach Sasamori at [log in to unmask]
or 847-615-7100 ext.2815
-----------------------------------------------------
Export Notice: This email may contain technical data controlled under the International Traffic in Arms Regulations (ITAR) by the U.S. Department of State (22 CFR 120-130) or under the U.S Export Administration Regulations (EAR) by the Department of Commerce (15 CFR 730-744). Violations of these export laws are subject to severe criminal penalties.
Legal Notice: This electronic message contains information from Carlisle Interconnect Technologies that may be privileged and confidential. The information is intended to be for the use of the individual(s) or entity named above. If you are not the intended recipient, be aware that any disclosure, copying, distribution or use of the contents of this information is prohibited. If you have received this electronic message in error, please notify us by telephone or e-mail (to the numbers or address above) immediately.
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 16.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
For additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|