Dave:
Given the fact that the DI water contains carbon dioxide (if only very small
amounts) I would expect attack, but the attack itself will change the water,
and neutralize the carbon dioxide, and stop further attack.
So, unless the water is being constantly refreshed, or worse, sprayed, (where
it can absorb more carbon dioxide), I would expect the attack to be at the
angstrom level.
And this is given an hour, heated. The use of DI water for rinsing, where it
has neglible contact time, seems wholly appropriate.
Rudy Sedlak
RD Chemical Company
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|