Hi Ken & All -
Check IPC-6012 -- in my recollection, Class 2 allows up to 90 degrees of
breakout.
Regards - Kelly
-----Original Message-----
From: Ken Patel <[log in to unmask]>
To: [log in to unmask] <[log in to unmask]>
Date: Wednesday, October 13, 1999 3:26 PM
Subject: Re: [TN] Reliability due to misregistration on inner layer
>Steve,
>Only things I can tell you is that we have a 90 degree break out. The
>material used was a 170 Tg on a 12 layer board. I don't know about any
>violation of minimum lines and spaces standards, is it something we should
>measure or expect our fab house to tell us?
>
>re,
>ken patel
>
>At 07:17 PM 10/12/1999 EDT, [log in to unmask] wrote:
>>In a message dated 10/12/99 5:51:38 PM Central Daylight Time,
[log in to unmask]
>>writes:
>>
>>> On one of our product, we have found that one of the inner layer has
>>> misregistration.
>>>
>>> Do you see any quality/ long term reliability problem associated with
inner
>>> layer misregistration? Our requirement was to have a 1 mil minimum
annular
>>> ring on all inner layers. What is the risk cum liability of accepting
those
>>> boards knowing that they are misregistered.
>>>
>>> Misregistration occurred at 1mm BGA where the finished hole diameter is
9
>>> mil on a 20 mil pads.
>>>
>>> re,
>>> ken patel
>>
>>Ken,
>>
>>As one who is learning, and one who has experienced some bare board
problems
>>recently, I would like to ask a question or two to clarify...
>>
>>1. Are you seeing break-out? No complete anular ring at all, just partial?
>>
>>2. What is the laminate material of the board? How many layers? Does this
>>mis-registration violate any other minimum lines and spaces standards? Or
is
>>it just a problem of incomplete anular pads?
>>
>>Thanks,
>>
>>-Steve Gregory-
>>
>>
>______________________________________________________
>Ken Patel Phone: (408) 490-6804
>1708 McCarthy Blvd. Fax: (408) 490-6859
>Milpitas, CA 95035 Beeper: (888) 769-1808
>
>##############################################################
>TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
>##############################################################
>To subscribe/unsubscribe, send a message to [log in to unmask] with following
text in
>the body:
>To subscribe: SUBSCRIBE TECHNET <your full name>
>To unsubscribe: SIGNOFF TECHNET
>##############################################################
>Please visit IPC web site (http://www.ipc.org/html/forum.htm) for
additional
>information.
>If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
>847-509-9700 ext.5365
>##############################################################
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
847-509-9700 ext.5365
##############################################################
|
|
|