In soldering with lead-based solders (i.e. HMP, >90%Pb) is it
essential to pretin the components lead with a high Pb alloy for
component leads that are Sn85/Pb15 or Sn80/Pb20 plated, Sn60/Pb40 or
Sn63/Pb37 coated, and what about gold-plated?
What are the pro's/con's of not pretinning, undestanding the
propensity of leads (Pb) and tins (Sn) to lower the melting
points..How much I am not sure ! Is there a distinct advantage OF
pretinning with Pb ?
One other note, the storage temps will be greater than 190degC.