TECHNET Archives

August 2012

TechNet@IPC.ORG

Options: Use Monospaced Font
Show HTML Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
"David D. Hillman" <[log in to unmask]>
Reply To:
TechNet E-Mail Forum <[log in to unmask]>, [log in to unmask]
Date:
Wed, 15 Aug 2012 21:23:44 -0500
Content-Type:
text/plain
Parts/Attachments:
text/plain (1 lines)
Hi Graham - the 100 uinch value is applicable to PTH technology solder 
joints, the limit for SMT technology solder joints is much lower. The 
issue is gold embrittlement which isn't just driven by the gold thickness, 
you also need to take into account the volume of solder for the joint and 
the time/temperature parameters - aka do you give the gold sufficient time 
to diffuse throughout the solder volume. The IPC JSTD-001 Handbook and the 
IPC-820 Handbook both have some good information on gold thickness/gold 
embrittlement topic.  Good Luck.

Dave Hillman
Rockwell Collins
[log in to unmask]




Graham Collins <[log in to unmask]> 
Sent by: TechNet <[log in to unmask]>
08/15/2012 02:15 PM
Please respond to
TechNet E-Mail Forum <[log in to unmask]>; Please respond to
<[log in to unmask]>


To
<[log in to unmask]>
cc

Subject
[TN] gold removal question - to remove or not?






Hello Technet

I'm in the midst of a debate about gold removal.  Our policy on component 
leads is to double dip tin all gold.  J-STD-001 says I do not have to do 
it if there is less than "2.54 ìm [100 ìin]" of gold, but is it realistic 
to operate on that basis?  For example, looking at an Airborne brand 
connector I find the spec sheet says that there will be 50 ìin gold, 
minimum. Which is not totally helpful as it does not tell me maximum.  I'm 
assuming given the price of gold that they aren't looking to put a lot 
more than the minimum on, but how controllable is the process?  Could we 
check the thickness once and assume we are safe?

 

(and as you can tell from my phrasing I'm of the more conservative camp on 
this one, still dipping the parts until proven wrong)

 

regards, 
 
Graham Collins 
Halifax Production Engineering 
(902) 873-2000 ext. 6215 

 

This message and any attachments are solely for the use of the individual 
or entity to which it is addressed and may contain information that is 
privileged or confidential or controlled technical data that is subject to 
the laws of Canada or the United States. If you are not the intended 
recipient, any disclosure, use or distribution of the information 
contained herein is prohibited. If you have received this communication in 
error, please notify the sender by reply e-mail and immediately delete 
this message and any attachments.

 


______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________



______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

ATOM RSS1 RSS2