Hi Waclaw,
It sounds like famous "black pad" phenomena and it has nothing with Kapton,
but with Nickel layer.
Powodzenia
Edeward
Edward Szpruch
Eltek Ltd
P.O.Box 159 ; 49101 Petah Tikva Israel
Tel ++972 3 9395050 , Fax ++972 3 9309581
e-mail [log in to unmask]
> -----Original Message-----
> From: karpinski [SMTP:[log in to unmask]]
> Sent: ã ôáøåàø 18 2004 23:15
> To: [log in to unmask]
> Subject: [TN] Ni/Au solderability on kapton
>
> Recently we have solderability problems with Ni/Au kapton flex boards
> (0,1 µm Au, 3 µm Ni, 35m Cu).
> We have produced and assembled large number of boards.
> On 10 % of the boards we observe interconnection failures after final
> assembly of the pcbs. If the suspected solder joints are lightly
> stressed , the connections are easily broken, leaving an open circuits.
> It is easy to peel these parts with solder material from the boards.
> The pads below the removed parts are discolored dark gray and are sleek .
> Some times the handsoldering of the broken joins was successful but
> after small strain the joints broke again.
> Additional vapor phase soldering did not improved the the strength of
> the joints.
> This is new problem for us. Does anyone have any experience with this?
> How to rework the boards? How to determine when a board should be
> reworked or
> scrapped? What about reliability issues? Latent failures?
> I would appreciate your help very much
> regards
>
> --
> Waclaw Karpinski
> I. Physikalisches Institut
> RWTH Aachen
> D - 52074 Aachen
>
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 1.8e
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail to
> [log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to
> [log in to unmask]: SET Technet Digest
> Search the archives of previous posts at: http://listserv.ipc.org/archives
> Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
> for additional information, or contact Keach Sasamori at [log in to unmask] or
> 847-509-9700 ext.5315
> -----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
|
|
|