Mitch,
	Half ounce is designated with an "H".  I would also recommend 
specifying HTE copper foil since it more reliable and seems to be the 
standard.  In that case, for HTE half over half, it would be "HH/HH"

Glenn Pelkey
Maxtek Components corp.


[log in to unmask] (Mitch Morey) Wrote:
| 
| Help.
| 
| How do I call out 1/2oz Copper per MIL-P-13949? I know 
| it's C1/C1 for 1oz
| over 1 oz. What's 1/2?
| 
| Thanks,
| 
| Mitch Morey
| 
| **********************************************************
| *****************
| * TechNet mail list is provided as a service by IPC using 
| SmartList v3.05 *
| **********************************************************
| *****************
| * To subscribe/unsubscribe send a message <to: 
| [log in to unmask]>   *
| * with <subject: subscribe/unsubscribe> and no text in the 
| body.          *
| **********************************************************
| *****************
| * If you are having a problem with the IPC TechNet forum 
| please contact   *
| * Dmitriy Sklyar at 847-509-9700 ext. 311 or email at 
| [log in to unmask]      *
| **********************************************************
| *****************
| 
| 

***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To subscribe/unsubscribe send a message <to: [log in to unmask]>   *
* with <subject: subscribe/unsubscribe> and no text in the body.          *
***************************************************************************
* If you are having a problem with the IPC TechNet forum please contact   *
* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask]      *
***************************************************************************


ATOM RSS1 RSS2