TECHNET Archives

December 2004

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Content-Type:
text/plain; charset="us-ascii"
Sender:
Subject:
From:
Date:
Fri, 3 Dec 2004 08:23:30 -0500
MIME-Version:
1.0
X-To:
TechNet E-Mail Forum <[log in to unmask]>, Shahed Safavi-Bayat <[log in to unmask]>
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, [log in to unmask]
Parts/Attachments:
text/plain (157 lines)
Shahed,

Thanks for the correction.

Al




Shahed Safavi-Bayat <[log in to unmask]>
Sent by: TechNet <[log in to unmask]>
12/03/2004 08:03 AM
Please respond to TechNet E-Mail Forum; Please respond to Shahed
Safavi-Bayat


        To:     [log in to unmask]
        cc:
        Subject:        Re: [TN] Cpk calculation for registration


Al,
I believe formula needs to be modified as below since it misses "absolute"
value. Am I correct?

cpk = abs(mean - closest_limit) / (3 * sigma)
abs = absolute value
mean = average of the measurements
sigma = standard deviation


Best Regards,

Shahed


-----Original Message-----
From: [log in to unmask] [mailto:[log in to unmask]]
Sent: Friday, December 03, 2004 7:52 AM
To: [log in to unmask]
Subject: Re: [TN] Cpk calculation for registration


Parial,

Don't know enough about your process, but from a statistical point of
view, simply - Cpk is equal to the distance from the process mean to the
nearest spec limit divided by three times the standard deviation:

Cpk= (process mean - nearest spec limit) /  (3 std. dev)

That being said, Cpk should always be greater than 1.0, or you have a
problem.

So, if you can measure the registration of the drilled holes, and have a
spec, you're set to go.

Good luck,

Al Kreplick
Sr. Mfg. Eng.
Teradyne, Inc.
500 Riverpark Drive
Mail Stop NR500 1-1
North Reading, MA 01864
Tel: 978-370-1726





Parial Swati <[log in to unmask]>
Sent by: TechNet <[log in to unmask]>
12/02/2004 11:06 PM
Please respond to TechNet E-Mail Forum; Please respond to Parial Swati


        To:     [log in to unmask]
        cc:
        Subject:        [TN] Cpk claculation for registration


Dear friends,
Any ideas about the ways to calculate the Cpk value for registration of
the
drilled holes with the inner layers.

Regards,
Swati...

Scan by AT&S virus protection

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask]
or 847-615-7100 ext.2815
-----------------------------------------------------



---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask]
or 847-615-7100 ext.2815
-----------------------------------------------------

--
No virus found in this incoming message.
Checked by AVG Anti-Virus.
Version: 7.0.289 / Virus Database: 265.4.5 - Release Date: 12/3/2004


--
No virus found in this outgoing message.
Checked by AVG Anti-Virus.
Version: 7.0.289 / Virus Database: 265.4.5 - Release Date: 12/3/2004


---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask]
or 847-615-7100 ext.2815
-----------------------------------------------------



---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2