The DSC usually gave high Tg value than TMA.
jk
At 08:41 AM 4/20/99 PDT, you wrote:
>Hello all,
>
>Could somebody tell me how the measurement results differ? I vaguely
>recall that when measuring the same board by these two different
>methods, one method would show a slightly higher value than the other.
> But, I can't recall which one. For example, is 135 C Tg by DSC
>equivalent to 130 C Tg by TMA?
>
>I know there's sample and test variation, but I'm looking at results
>in general.
>
>And, while we're on it, which test method is your preference,
>especially when it comes to specification issues.
>
>Thanks
>
>Glenn Pelkey
>[log in to unmask]
>[log in to unmask]
>
>
>
>_______________________________________________________________
>Get Free Email and Do More On The Web. Visit http://www.msn.com
>
>################################################################
>TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
>################################################################
>To subscribe/unsubscribe, send a message to [log in to unmask] with following
text in the body:
>To subscribe: SUBSCRIBE TechNet <your full name>
>To unsubscribe: SIGNOFF TechNet
>################################################################
>Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section
for additional information.
>For technical support contact Hugo Scaramuzza at [log in to unmask] or
847-509-9700 ext.312
>################################################################
>
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################
|
|
|