TECHNET Archives

September 2005

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
John Burke <[log in to unmask]>
Reply To:
TechNet E-Mail Forum <[log in to unmask]>, John Burke <[log in to unmask]>
Date:
Mon, 12 Sep 2005 15:34:36 -0700
Content-Type:
text/plain
Parts/Attachments:
text/plain (98 lines)
Were those shipped from the board vendor like that or were they put through
a reflow cycle unpopulated?

John
------------------------------------
Avanex
John Burke
Senior Manager RoHS Compliance
[log in to unmask]
40919 Encyclopedia Circle
Fremont
CA 94538
tel: 510 897 4250
fax: 510 979 0189
mobile: 510 676 6312
------------------------------------


-----Original Message-----
From: TechNet [mailto:[log in to unmask]]On Behalf Of Brooks,Bill
Sent: Monday, September 12, 2005 2:54 PM
To: [log in to unmask]
Subject: [TN] raised vias...


Can someone give us a read on what they think cause the raised vias on
Steve's website picture? http://www.stevezeva.homestead.com  page 2.


Bill Brooks - KG6VVP
PCB Design Engineer, C.I.D.+, C.I.I.
Tel: (760)597-1500 Ext 3772 Fax: (760)597-1510
Datron World Communications, Inc.
_______________________________________
San Diego Chapter of the IPC Designers Council
Communications Officer, Web Manager
http://dcchapters.ipc.org/SanDiego/
http://pcbwizards.com

-----Original Message-----
From: Steve Gregory [mailto:[log in to unmask]]
Sent: Monday, September 12, 2005 2:28 PM
To: [log in to unmask]
Subject: Re: [DC] Raised vias

Hi Fred and Everybody!

Speaking of "Raised Vias" and "Anthills", I have some anthills on some
Boards that we're building here now.

The anthills aren't from plugging or anything, but are blind via in pad.

I thought that they wouldn't present too much of a problem because I
thought that after printing paste and reflow, everything would level
out...but that wasn't the case.

At locations where I was placing something called a PowerPAK SO8, there was
open solder defects at some of the joints because (I think) of the raised
vias. You can see the PowerPAK part drawing, and the raised vias that I'm
talking about on my web page at: http://www.stevezeva.homestead.com . Go to
"Picture Page 2" and look for "PowerPAK SO8 and Raised Vias".

I don't have a clue why the vias are raised like that...maybe that's a
question for the TechNet.

Kind regards,

-Steve Gregory-
Senior Process Engineer
LaBarge Incorporated
Tulsa, Oklahoma
(918) 459-2285
(918) 459-2350 FAX

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2