Hi Roger,
There are some results on this in IPC-TR-579 "Round Robin Reliability
Evaluation of Small Diameter Plated Through Holes in Printed Wiring Boards."
There is indication, that the no-functional lands provide a very moderate
reliability improvement, but that any decrease in quality due to the more
difficult manufacturing processes might negate this benefit.
...and the MoonMan is absolutely correct when he writes:
>Your desire to save real estate is a good one. Just make sure the copper
>thickness is there and the ductility is high.
He is talking abouit 1.5 mils, not 0.8 mils of copper in the PTV; if you get
thin pating, the thermal expansion of the resin during any soldering process
will plastically bulge the copper barrel walls inward and create a space
between the barrel walls and the resin hole after shrinking during cooling.
Werner Engelmaier
Engelmaier Associates, L.C.
Electronic Packaging, Interconnection and Reliability Consulting
7 Jasmine Run
Ormond Beach, FL 32174 USA
Phone: 386-437-8747, Fax: 386-437-8737
E-mail: [log in to unmask], Website: www.engelmaier.com
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|