James,
This e-mail jogged my memory, so I dug into my archives and came up with a
reference in JPL Des Req DM509306 C, Vol 1 paragraph 3.4.5.4.2.f. (issue
date 1 September 1978) which supports the notion of making a rounded joint
(smooth solder ball) with no sign of the lead or terminal showing through.
Regards,
Phil Nutting
Manufacturing Engineer
Kaiser Systems, Inc.
-----Original Message-----
From: Terveen, James @ NARDAEAST
[mailto:[log in to unmask]]
Sent: Wednesday, October 25, 2000 9:22 AM
To: [log in to unmask]
Subject: Re: [TN] Ball soldering for high voltage PCB assembly
I know that NASA training used to have a section on how to solder high
voltage connection in there training. If someone out there has some
information from that it may help you
-----Original Message-----
From: Joel Miller [mailto:[log in to unmask]]
Sent: Wednesday, October 25, 2000 8:25 AM
To: [log in to unmask]
Subject: [TN] Ball soldering for high voltage PCB assembly
I am new to this list.
I am looking for information pertaining to Ball Soldering for high voltage
PCB assembly.
Is there a IPC standard or a procedure on how to do this technique?
Joel Miller
----------------------------------------------------------------------------
-----
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
Search previous postings at: www.ipc.org > On-Line Resources & Databases >
E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
----------------------------------------------------------------------------
-----
----------------------------------------------------------------------------
-----
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
Search previous postings at: www.ipc.org > On-Line Resources & Databases >
E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
----------------------------------------------------------------------------
-----
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|